Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 177 MPa | 25600 psi | ASTM D638 |
Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced Nylon 6, 20% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Tensile Strength, Yield | 177 MPa | 25600 psi | ASTM D638 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Tensile Strength, Yield | 177 MPa | 25600 psi | ASTM D638 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 177 MPa @Thickness 3.20 mm |
25600 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol) Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG .. |
|||
Tensile Strength, Yield | 177 MPa @Thickness 3.20 mm |
25600 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 177 MPa @Thickness 3.20 mm |
25600 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 177 MPa @Thickness 3.20 mm |
25600 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | >= 177 MPa | >= 25600 psi | |
Saint-Gobain Norslide® EKO-V PTFE Sliding Tubing Features/Benefits:Low stick-slip effectMaintenance free, no lubrication requiredWeatherproofIsolates noise, dampens vibrationFlexible and resilientResistant against fuel, oil, and greasesService tem.. |
|||
Tensile Strength, Yield | 177 MPa | 25600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140C PPS Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 177 MPa | 25600 psi | ASTM D638 |
Cheng Yu Plastic FR200GV45 Flame Retardant Nylon 66, 45% Glass Fiber |
|||
Tensile Strength, Yield | 177 MPa | 25600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140C PPS Information provided by Samsung Cheil Industries. |