Polymer Property : Tensile Strength, Yield = 25500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 176 MPa
25500 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE  (discontinued **)
Data provided by PolyOne.
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Tensile Strength, Yield 176 MPa

@Strain 0.200 %,
Temperature 538 °C
25500 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes HR-160® alloy, hot rolled and solution annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Yield >= 176 MPa

@Strain 0.200 %,
Temperature 249 °C
>= 25500 psi

@Strain 0.200 %,
Temperature 480 °F
H.C. Starck Ultra 76 Alloy (Ta 2.5%W)
Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low..
Tensile Strength, Yield 176 MPa
25500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP LFL36E PEEK
LNP* LUBRICOMP* LFL36E is a compound based on Polyetheretherketone containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Wear Resistant, Easy Molding.
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES Elastoblend® PA6 GF40 IM HS UV RD 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES Elastoblend® PA6 GF43 IM L BKN 43% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 HS BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 HS L BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 HS UV 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 L BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 L N BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 L UV 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 RM BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low Moisture AbsorptionAppearance: BlackTPCI# 9719102Information provided by T..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF30 UV BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedAppearan..
Tensile Strength, Yield 176 MPa
25500 psi
ASTM D638
Techmer ES HiFill® PA6 GF33 HS BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedAppearanc..
Tensile Strength, Yield 176 MPa
25500 psi
Saint-Gobain Rulon® II Bearing/Seal PTFE
An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al..
Tensile Strength, Yield 176 MPa
25500 psi
.0275 - .035 inches sheet thickness; ASTM A 370
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel
Tensile Strength, Yield 176 MPa
25500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON OE003A PPS - BRANCHED (Europe-Africa-Middle East)
LNP* STATKON* OE003A is a compound based on PPS ( branched ) resin containing Carbon Fiber. Added features include: Electrically Conductive.