Polymer Property : Tensile Strength, Yield = 25.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.1 MPa
3640 psi
ASTM D638
Multibase Multi-Pro® 4012 X Platinum Polypropylene
Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase
Tensile Strength, Yield 25.1 MPa
3640 psi
ASTM D638
Ravago Manufacturing Americas Echo® RPEHD NAT Recycled HDPE
Recycled High Density Polyethylene, Natural Color, Fractional Melt FlowInformation provided by Ravago.
Tensile Strength, Yield 25.1 MPa

@Thickness 3.20 mm
3640 psi

@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Pinnacle Polymers 2135 Impact Polypropylene Copolymer, Injection Molding Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Tensile Strength, Yield 25.1 MPa
3640 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Hi-Sil 233 Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 25.1 MPa
3640 psi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tensile Strength, Yield 25.1 MPa
3640 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Hi-Sil 233 Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 25.1 MPa
3640 psi
ISO 527-2/50
ExxonMobil AP03B Polypropylene Impact Copolymer
Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio..
Tensile Strength, Yield 25.1 MPa
3640 psi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..