Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.63 MPa | 237 psi | 200%, post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.63 MPa | 237 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7272 Butyl and Halobutyl Rubber General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | >= 1.63 MPa | >= 237 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7345 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |