Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.1 MPa | 2190 psi | ASTM D412 |
Precision Polymer Engineering V70B Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature. |
|||
Tensile Strength, Yield | 15.1 MPa | 2190 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMU 130 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Europe F.. |
|||
Tensile Strength, Yield | 15.1 MPa | 2190 psi | Molded property |
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and.. |