Mechanical Properties Metric English Comments
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified
Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Tensile Strength, Yield 141 MPa

@Temperature 149 °C
20500 psi

@Temperature 300 °F
ASTM D638
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled  (discontinued **)
AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU..
Tensile Strength, Yield 141 MPa

@Temperature 149 °C
20500 psi

@Temperature 300 °F
ASTM D638
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled  (discontinued **)
AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU..
Tensile Strength, Yield 141 MPa
20500 psi
ISO 527
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber
Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical ..
Tensile Strength, Yield 141 MPa
20500 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear
LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for..
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Techmer ES HiFill® PA6 GF20 L 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength, Yield 141 MPa
20500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT
LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Techmer ES HiFill® PBT GF30 HR BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Hydrolysis ResistantAppearance: BlackInformation provided by TP Composites, In..
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Techmer ES HiFill® PVDF CF15 BK 15% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Techmer ES HiFill® R60 G33-L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorTPCI# 9208102Information..
Tensile Strength, Yield 141 MPa
20500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific)
LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006.
Tensile Strength, Yield 141 MPa
20500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific)
LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006.
Tensile Strength, Yield 141 MPa
20500 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC
LNP* THERMOCOMP* DC006H is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
Tensile Strength, Yield 141 MPa
20500 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC (Asia Pacific)
LNP* Thermocomp* DC006H is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Techmer ES Plastiblend® PBT/ABS GF30 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Techmer ES Elastoblend® PA6/6 GF33 IM HS L BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
Tensile Strength, Yield 141 MPa
20500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DEL359EF PC
LNP* STAT-KON* DEL359EF is a compound based on Polycarbonate containing 25% Carbon Fiber, 15% PTFE. Added features include: Flame Retardant. Electrically Conductive, Wear Resistant.
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Techmer ES HiFill® PBT G/CF30 IM 15% Glass/Carbon Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInform..
Tensile Strength, Yield 141 MPa
20500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive)
Non-sloughing carbon-fiber-filled material with resistance to most chemicals and solvents mechanically strong and tough, thermally stable to 335F, flame and abrasion resistant, and easily fabricated..
Tensile Strength, Yield 141 MPa
20500 psi
5 mm/min; ISO 527
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded
RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar.
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Ashley Polymers Ashlene® 525-33G Nylon 66, 33% Glass Reinforced
High impact Nylon 66 reinforced with 33% glass fibers, lubricated.Data provided by the manufacturer
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Cheng Yu Plastic A707G25 SAN, 25% Glass Fiber