Polymer Property : Tensile Strength, Yield = 2.41 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.41 MPa
350 psi
Mean Value, Flatwise, Core Failure, 39-42% RC; ASTM C297
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 3K PW G30-500 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Tensile Strength, Yield 2.41 MPa
350 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 584 Perfluoroelastomer
Greene Tweed’s Chemraz® 584, a cream-colored perfluoroelastomer, is a specialty compound formulated to outlast the most demanding chemical process applications. Because of its outstanding o..
Tensile Strength, Yield 2.41 MPa
350 psi
@100% Elongation; ASTM D1414
Greene Tweed Xyfluor® 860 Fluorinated Elastomer Compound
Xyfluor® 860, a highly fluorinated elastomer compound, offers excellent chemical compatibility over a wide range of temperatures from -76°F to 450°F (-60°C to 232°C). Recommended for..
Tensile Strength, Yield 2.41 MPa
350 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 570 Perfluoroelastomer
Chemraz® 570, recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control is required, offers excellent perfor..
Tensile Strength, Yield 2.41 MPa
350 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 640 Perfluoroelastomer
Chemraz® 640 perfluoroelastomer is specifically developed by Greene Tweed to meet the rigorous demands of aggressive plasma systems. This product’s unique formulation provides enhanced plas..
Tensile Strength, Yield >= 2.41 MPa
>= 350 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7182D Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.41 MPa

@Strain 300 %
350 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1843L1 Thermoplastic Elastomer
Notes: Translucent Features: High FlowInformation Provided by Teknor Apex
Tensile Strength, Yield 2.41 MPa
350 psi
Transverse/Width
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.004" thick)
Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation..
Tensile Strength, Yield 2.41 MPa
350 psi
Transverse/Width
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.005" thick)
Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation..
Tensile Strength, Yield 2.41 MPa
350 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3720 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding..