Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 191 MPa | 27700 psi | ASTM D638 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR33 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | SABIC - Japan Method |
SABIC Innovative Plastics Lexan® LC120 PC (Asia Pacific) |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | ISO 527 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | ASTM D638 |
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Tensile Strength, Yield | 191 MPa @Thickness 3.20 mm |
27700 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 191 MPa @Thickness 3.20 mm |
27700 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | ASTM D638 |
Techmer ES HiFill® PA6 CF20 BK 20% Carbon Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 8738102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific) LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | ASTM D638 |
Ashley Polymers Ashlene® 528L-30LG Nylon 66, 30% Long Glass Fiber Reinforced Long glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provid.. |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Verton OX07411 PPS LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 191 MPa | 27700 psi | ASTM D638 |
Samyang Tripet® 2500G45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information.. |