Mechanical Properties Metric English Comments
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
PolyOne OnForce™ LFT NN-30 LGF/000 Natural Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced
Nylon 66, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Tensile Strength, Yield 183 MPa
26500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ PK-30CF/15T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated  (discon
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Polymer Resources NY66-G33-[color]-H Nylon 66, 33% Glass Reinforced, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Tensile Strength, Yield 183 MPa
26500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon EE008E PEI
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r..
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PA6 GF33 L N BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: Fast Molding Cycle and LubricatedAppearance: BlackTPCI# 87..
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PA6 GF40 L 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PA6 GF40 L BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Comp..
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF30 HS L BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc..
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF30 L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF30 LE 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF33 LE BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesAppearance: BlackTPCI#7762101Information provided by TP Compos..
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF33 SF L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Strontium FerriteFeatures: LubricatedInformation provided by TP ..
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Techmer ES HiFill® PEEK GF30 HF 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc.
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Ashley Polymers Ashlene® 980LS-43GB Nylon 612, 43% Glass Reinforced
A 43% glass reinforced, heat stabilized Nylon 612 resin in black.Data provided by the manufacturer
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..