Polymer Property : Tensile Strength, Yield = 18.64 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.64 MPa
2704 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 18.64 MPa
2703 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 18.64 MPa
2703 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 18.64 MPa
2704 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..