Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 175 MPa | 25400 psi | ASTM D638 |
NYCOA 27/300SR Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 H-B nylon 6Information provided by NYCOA, Inc. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | ISO 527-1/-2 |
Lanxess Durethan® DP 2037/30 H2.0 LT 904040 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, black colored for laser transmission-welding (laser-transparent), good heat-ageing resistance |
|||
Tensile Strength, Yield | 175 MPa @Strain 0.200 %, Temperature 760 °C |
25400 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Yield | 175 MPa @Strain 0.200 %, Temperature 540 °C |
25400 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr.. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr.. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear.. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI (Asia Pacific) LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF006S is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V8090 PBT+PET (Europe-Africa-Middle East) 50% Glass Fiber Reinforced PBT-PET resin |
|||
Tensile Strength, Yield | >= 175 MPa @Strain 0.200 % |
>= 25400 psi @Strain 0.200 % |
|
Schmolz + Bickenbach UGICHROM 4307 Austenitic Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | ISO 527 |
Polyram PlusTek PA303G6BK16 Nylon 6.6, 30% Glass Fiber reinforced, Heat Stabilized, Hydrolysis Resistant 30% Glass fiber reinforced, heat stabilized, hydrolysis resistant, improved surface finish Nylon 6.6. Approved and listed by W.R.A.S.Information provided by Polyram. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | ASTM-D638 |
Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, UV stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | ASTM-D638 |
Polyram PlusTek PA4801G6 Nylon 6.6, 30% Glass Fiber Reinforced, PTFE lubricated 30% glass fiber reinforced, PTFE lubricated polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 175 MPa | 25300 psi | ASTM D638 |
Cheng Yu Plastic N6G35 Nylon 6, 35% Glass Filled |
|||
Tensile Strength, Yield | 175 MPa | 25400 psi | ASTM D638 |
Solvay TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY Description: Polyamide 6, 30% glass fiber reinforced, for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 1021GF6 is used in all sectors of industry, offering an excelle.. |