Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.0 - 117 MPa | 6090 - 17000 psi | Average value: 79.2 MPa Grade Count:14 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Tensile Strength, Yield | 51.7 - 117 MPa | 7500 - 17000 psi | Average value: 85.9 MPa Grade Count:32 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Tensile Strength, Yield | 21.4 - 117 MPa | 3100 - 17000 psi | Average value: 51.5 MPa Grade Count:20 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Tensile Strength, Yield | 55.2 - 117 MPa | 8000 - 17000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, Annealed CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Yield | 0.539 - 117 MPa | 78.2 - 17000 psi | Average value: 61.4 MPa Grade Count:12 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Tensile Strength, Yield | 110 - 117 MPa | 15900 - 17000 psi | Average value: 114 MPa Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Tensile Strength, Yield | 12.0 - 117 MPa @Temperature -40.0 - 120 °C |
1740 - 17000 psi @Temperature -40.0 - 248 °F |
Average value: 56.9 MPa Grade Count:8 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |