Polymer Property : Tensile Strength, Yield = 167 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 167 MPa

@Thickness 3.20 mm
24200 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUCON PO6062 mPPO+CNT+CF+GF
Description: Injection Molding, mPPO+CNT+CF+GF, High Strength, Heat StabilityApplication: ATM parts, LCD Cell TrayCAS No. 35134-01-4, 25038-54-4, 65997-17-3, 7440-44-0 and 7782-42-5Information provi..
Tensile Strength, Yield 167 MPa
24200 psi
ASTM D638
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Tensile Strength, Yield 167 MPa
24200 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66
LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant.
Tensile Strength, Yield 167 MPa
24200 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific)
LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Tensile Strength, Yield 167 MPa
24200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 167 MPa
24200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 167 MPa
24200 psi
ASTM D638
Cheng Yu Plastic N6G20 Nylon 6, 20% Glass Filled
Tensile Strength, Yield 167 MPa
24200 psi
ASTM D638
Cheng Yu Plastic N6GV30 Flame Retardant Nylon 6, 30% Glass Filled