Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1.13 MPa | >= 164 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 4503 Natural Rubber General purpose Natural RubberInformation provided by Seals Eastern, Inc. |