Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 158 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 158 - 188 MPa
22900 - 27300 psi
Average value: 168 MPa Grade Count:4
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Tensile Strength, Yield 158 MPa
22900 psi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Tensile Strength, Yield 158 MPa

@Strain 0.200 %
22900 psi

@Strain 0.200 %
Materion AlBeCastâ„¢ IC910 Aluminum Beryllium Composite
Mechanical properties are typical values at RT. AlBeCastâ„¢ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stif..
Tensile Strength, Yield 158 MPa
22900 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2310EPR PEI
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Tensile Strength, Yield 158 MPa
22900 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Tensile Strength, Yield 158 MPa
22900 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing.
Tensile Strength, Yield 158 MPa
22900 psi
5 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r..
Tensile Strength, Yield 158 MPa
22900 psi
5 mm/min; ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..
Tensile Strength, Yield 158 MPa
22900 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF35 L UV 35% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi..
Tensile Strength, Yield 158 MPa
22900 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East)
LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
Tensile Strength, Yield 158 MPa
22900 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK
LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber.
Tensile Strength, Yield 158 MPa
22900 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific)
LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Tensile Strength, Yield 158 MPa
22900 psi
ASTM D 638
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP
LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 158 MPa
22900 psi
ISO 527
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP
LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength, Yield 158 MPa
22900 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific)
LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.
Tensile Strength, Yield 158 MPa
22900 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific)
LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.
Tensile Strength, Yield 158 MPa
22900 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Tensile Strength, Yield 158 MPa
22900 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Tensile Strength, Yield 158 MPa
22900 psi
ISO 527-2/1A/5
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret..
Copyright © lookpolymers.com All Rights Reserved