Polymer Property : Tensile Strength, Yield = 155 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.07 MPa
155 psi
at 200%, as molded
Multibase SILASTIC® C7-4535 DICUP R Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.07 MPa
155 psi
at 200%, as molded
Multibase SILASTIC® C7-4535 TBPB Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 1.07 MPa
155 psi
at 150% Elongation, maximum
Dow Corning SILASTIC® LCS-740 SILICONE RUBBER
40 Durometer, translucent, low compression set, uncatalysed Silicone Rubber Base suitable for molding.Information provided by Dow Corning