Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 80.0 - 152 MPa | 11600 - 22000 psi | Average value: 124 MPa Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Tensile Strength, Yield | 89.6 - 152 MPa | 13000 - 22000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, Annealed Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |