Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 62.1 - 103 MPa | 9000 - 14900 psi | Average value: 81.0 MPa Grade Count:8 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Tensile Strength, Yield | 14.8 - 103 MPa | 2150 - 14900 psi | Average value: 46.3 MPa Grade Count:363 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Yield | 30.0 - 103 MPa | 4350 - 14900 psi | Average value: 72.4 MPa Grade Count:24 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |