Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.51 MPa | 1380 psi | ASTM D412 |
Polymax® Maxelast® P3875 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | ASTM D412 |
Precision Polymer Engineering S70X Silicone Rubber Red Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Specially compounded to provide .. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | ASTM D412 |
Precision Polymer Engineering S75T Silicone Rubber Translucent Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. Silicone compound in conformity with.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | ASTM D638 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | ASTM D638 |
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress .. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | ISO 527-2 |
Carmel Olefins IPETHENE® 800 Low Density Polyethylene
(discontinued **) IPETHENE® 800 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits high flow and flexibility. APPLICATIONS IPETHENE® 800 i.. |
|||
Tensile Strength, Yield | 9.50 - 170 MPa | 1380 - 24600 psi | Average value: 45.8 MPa Grade Count:321 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | |
Kraton® D1102 + LDPE blend (6/94) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | 300% Elongation; ASTM D412 |
SPS Guang Zhou POFLEXâ„¢ EP8300 Cable Grade TPU Non-halogen flame-retarded TPU material TPU POFLEXâ„¢ EP8300 is used to produce wire and cable. Halogen-free with good flammability and excellent mechanical property and heat resistance.Informat.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | 500 mm/min; GOST 11262 |
Sibur 15803-020 Low Density Polyethylene For production of films and film articles, including thermoset films, thin films, food contact grade films
(including tight packing), general-purpose films, and bags. |
|||
Tensile Strength, Yield | 9.51 MPa | 1380 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3085-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength, Yield | 9.51 MPa | 1380 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098A-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | ASTM D638 |
Chevron Phillips Marlex® 1122B Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Excellent Flexibility, Moderate Flow, Moderate Warping Resistance, Moderate Mold Release, Excellent ESCRApplicati.. |
|||
Tensile Strength, Yield | 9.50 MPa @Strain 300 % |
1380 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® W DP 85786A Polyurethane Grade for calanderingno yellowing under the action of UV lightgood low-temperature flexibilityhigh rebound resilienceimproved microbial resistanceImproved hydrolysis resistanceApplicationTextile coa.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | |
Dow LDPE 640IM Low Density Polyethylene DOW LDPE 640IM resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate stiffness for general purpose, and cap.. |
|||
Tensile Strength, Yield | 9.50 MPa | 1380 psi | Molded property |
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Tensile Strength, Yield | 9.51 MPa | 1380 psi | ASTM D-638 |
Axiall 10705 Wire & Cable Flexible PVC Non-lead stabilized general purpose 75C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf.. |
|||
Tensile Strength, Yield | 9.51 MPa | 1380 psi | ASTM D-638 |
Axiall 10702 Wire & Cable Flexible PVC General purpose 80°C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
Tensile Strength, Yield | 9.51 MPa | 1380 psi | ASTM D638 |
M. Holland Company LD400 LDPE
(discontinued **) Features: High ESCR (Stress Crack Resist.), Good Processability, Low Temp. StrengthUses: Closures, Electrical Parts, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 2.3Processing Method: Injection .. |