Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 13.4 MPa | 1940 psi | ASTM D412 |
Polymax® Maxelast® P3885H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 13.4 MPa | 1940 psi | ASTM D638 |
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Tensile Strength, Yield | 13.4 MPa | 1940 psi | ASTM D412 |
Polymax® Maxelast® C4885 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 13.4 MPa | 1950 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® 1047-0000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Tensile Strength, Yield | 13.4 MPa | 1940 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3210-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 13.4 MPa | 1950 psi | ASTM D412 |
Teknor Apex APEX® 3311-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 13.4 MPa | 1950 psi | ASTM D412 |
Teknor Apex APEX® 90-P513A-60-NT Polyvinyl Chloride+PUR Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | >= 13.4 MPa | >= 1950 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7182A Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. Resistant to extrusion. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 13.4 MPa | 1950 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Hi-Sil 233 Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 13.4 MPa | 1950 psi | ASTM D-638 |
Axiall 10801 Wire & Cable Flexible PVC Jacket compound recommended for 80°C maximum service temperature at a minimum wall thickness of 30 mils. UL recognized for 720 hour sunlight resistance.Information provided by Georgia GulfGeorgia .. |
|||
Tensile Strength, Yield | 13.4 MPa | 1950 psi | ASTM D-638 |
Axiall 8745 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 13.4 MPa | 1950 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Hi-Sil 233 Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |