Polymer Property : Tensile Strength, Yield = 1183 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.156 MPa
1183 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 2870 Thermoplastic Elastomer
Elastocon® 2870 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2870 is FDA compliant and well suited for cons..
Tensile Strength, Yield 8.158 MPa
1183 psi
302°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..