Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Tensile Strength, Yield | 78.6 MPa | 11400 psi | ASTM D 638 |
LyondellBasell Hostacomâ„¢ BJ23A Polypropylene Copolymer Description: Hostacomâ„¢ BJ23A is a polypropylene copolymer that is used for appliance componentsFeatures: Good StiffnessGood FlowChemically CoupledGood Impact ResistanceInformation provided by B.. |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 78.6 MPa | 11400 psi | ASTM 638 |
PlastxWorld CEVIAN® VGR20 20% GF ABS Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | ASTM D638 |
Cheng Yu Plastic N6CV3 Flame Retardant Nylon 6, 30% Mineral Reinforced |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | ASTM D638 |
Cheng Yu Plastic T882GV1 Flame Retardant PBT, 10% Glass Fiber |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | ASTM D638 |
Cheng Yu Plastic T888G1 PBT, 10% Glass Fiber |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | ASTM D638 |
Cheng Yu Plastic FRCV100 Flame Retardant Nylon 66, 10% Mineral Reinforced |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 78.5 MPa | 11400 psi | ASTM D638 |
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr.. |
|||
Tensile Strength, Yield | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Tensile Strength, Yield | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |