Mechanical Properties Metric English Comments
Tensile Strength, Yield 1062 MPa

@Strain 0.200 %
154000 psi

@Strain 0.200 %
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..
Tensile Strength, Yield 1062 MPa

@Strain 0.200 %
154000 psi

@Strain 0.200 %
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Longitudinal Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Tensile Strength, Yield 1062 MPa

@Strain 0.200 %
154000 psi

@Strain 0.200 %
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Transverse Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..