Mechanical Properties Metric English Comments
Tensile Strength, Yield 1060 - 1170 MPa
154000 - 170000 psi
Solution Annealed & Aged
Materion Beryllium Copper Alloy 245C Castings (UNS C82600)
Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula..
Tensile Strength, Yield 1060 - 1380 MPa
154000 - 200000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200)
Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Yield 1060 - 1350 MPa
154000 - 196000 psi
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17200)
Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi..
Tensile Strength, Yield 1060 - 1350 MPa
154000 - 196000 psi
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200)
Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi..
Tensile Strength, Yield 1060 - 1350 MPa
154000 - 196000 psi
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300)
Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi..
Tensile Strength, Yield 1060 - 1210 MPa
154000 - 175000 psi
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM08 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R..
Tensile Strength, Yield 1060 - 1170 MPa
154000 - 170000 psi
Solution Annealed & Aged
Materion Beryllium Copper Alloy 245CT Castings (UNS C82600)
Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula..
Tensile Strength, Yield 1060 MPa

@Strain 0.200 %
154000 psi

@Strain 0.200 %
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..