Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.45 MPa | 210 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.45 MPa | 210 psi | at 200%, as molded |
Multibase SILASTIC® C7-4535 VAROX Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.45 MPa | 210 psi | at 100%; ASTM D412 |
PB1100-60 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 1.45 MPa | 210 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.45 MPa | 210 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | >= 1.45 MPa | >= 211 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5722 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.45 MPa | 210 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7075 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |