Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.896 MPa | 130 psi | at 200%, no post cure- press cured for 5 minutes; ASTM D412 |
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 0.896 MPa | 130 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5401 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 0.896 MPa | 130 psi | ASTM D412 |
Saint-Gobain COHRlastic® R10470 Firm General-Purpose Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Tensile Strength, Yield | 0.896 MPa | 130 psi | ASTM D-412 |
Saint-Gobain Normount® V4600 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive Description: Ideal for Exterior Mounting Applications: Normount® V2800/V4600 closed-cell foam bonding tapes are highly conformable. The foam substrate allows energy and stress in the joint to be .. |
|||
Tensile Strength, Yield | 0.896 MPa | 130 psi | ASTM D-412 |
Saint-Gobain T-Bond II® Semi-Rigid Polyurethane Foam Structural Glazing and Cladding Spacer System Description: Semi-Rigid Polyurethane Foam Substrate used as a Structural Glazing and Cladding Spacer System for In-Shop Fabrication. Semi-Rigid Polyurethane: An open cell structure allows air and mo.. |
|||
Tensile Strength, Yield | 0.896 MPa | 130 psi | ASTM D-412 |
Saint-Gobain Normount® V2800 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive Description: Ideal for Exterior Mounting Applications: Normount® V2800/V4600 closed-cell foam bonding tapes are highly conformable. The foam substrate allows energy and stress in the joint to be .. |
|||
Tensile Strength, Yield | 0.896 MPa | 130 psi | at 100%; ASTM D412 |
G-2706 Styrene-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 0.896 MPa @Strain 300 % |
130 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3730 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |