Polymer Property : Tensile Strength, Yield = 0.414 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.414 MPa
60.0 psi
at 200%, no post cure- press cured for 5 minutes; ASTM D412
Multibase C6-515 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 0.414 MPa
60.0 psi
ASTM D3574
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi..
Tensile Strength, Yield 0.414 MPa
60.0 psi
AAMA 810.1
Saint-Gobain Norton® V980 Paper Liner Pressure Sensitive Adhesive Foam Sealant
Description: Closed cell PVC foam with a pressure-sensitive adhesive on both sides. Proven Performance: Norseal® V980/V990 foam sealant combines a closed cell polyvinyl chloride foam substrate wt..
Tensile Strength, Yield 0.414 MPa
60.0 psi
AAMA 810.1
Saint-Gobain Norton® V990 Poly Liner Pressure Sensitive Adhesive Foam Sealant
Description: Closed cell PVC foam with a pressure-sensitive adhesive on both sides. Proven Performance: Norseal® V980/V990 foam sealant combines a closed cell polyvinyl chloride foam substrate wt..
Tensile Strength, Yield 0.414 MPa

@Strain 300 %
60.0 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1798 Thermoplastic Elastomer
Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly..
Tensile Strength, Yield 0.414 MPa
60.0 psi
at 150% elongation, maximum
Dow Corning 1437 INDUSTRIAL SEALANT AND ADHESIVE
Neutral Cure RTV SealantInformation provided by Dow Corning
Tensile Strength, Yield 0.414 MPa
60.0 psi
ASTM D3574
Saint-Gobain Korel® K40-35 Medium Deflection Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..