Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.410 MPa | 59.5 psi | at 50% Extension (0.5 x 0.38 x 2 in bead) |
Momentive Performance Materials Ultraglaze® 4000 Construction Sealant High strength, one-part structural glazing/weathersealing system. Cure Method: Alkoxy (Neutral). Tack-free time 2 to 5 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Sili.. |
|||
Tensile Strength, Yield | 0.410 MPa | 59.5 psi | at 50% Extension (0.5 x 0.38 x 2 in bead) |
Momentive Performance Materials Ultraglaze® SSG 4000AC Construction Sealant High strength, one-part, accelerated-cure structural glazing/weathersealing system.Cure Method: Alkoxy (Neutral). Tack-free time 1 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silico.. |