Tensile Strength, Yield 0.0345 MPa
5.00 psi
TM R050-36
Resinlab® UR3001HP Black Urethane Encapsulant
Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e..
Tensile Strength, Yield 0.0345 - 11.7 MPa
5.00 - 1700 psi
Average value: 1.32 MPa Grade Count:17
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Tensile Strength, Yield 0.0345 MPa
5.00 psi
6 PCF
Unifrax Insulfrax® S Blanket Insulation
Insulfrax S Blanket is a flexible, strong, lightweight, needled blanket produced from Insulfrax Fiber. Mechanical needling of the spun Insulfrax fibers eliminates the need for binders in the produc..
Tensile Strength, Yield 0.0345 MPa
5.00 psi
TM R050-36
Resinlab® UR3001HP Clear Urethane Encapsulant
Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e..