Polymer Property : Film Tensile Strength at Break, MD = 9396 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 64.78 MPa
9396 psi
ASTM D882
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f..