Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | >= 58.6 MPa | >= 8500 psi | ASTM D 882 A |
Total Finathene® 2344 HDPE film
(discontinued **) Applications: Trash can liners, merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
LyondellBasell Alathon® L5005 High Density Polyethylene ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
Westlake Hifor Xtreme SC74844 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74844 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip, high antiblock and processing aid. Films produce.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
Westlake Hifor Xtreme SC74853 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74853 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and processing aid. Films produced wi.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
Westlake Hifor Xtreme SC74858 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74858 polymer is a high strength, good clarity linear low density polyethylene designed for blown film extrusion that contains no slip or antiblock and processing aid. Films .. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin Product Description: Enable 27-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
ExxonMobil LL 3003.32 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP) AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
Dow DOWLEX™ 2025G Linear Low Density Polyethylene DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp.. |
|||
Film Tensile Strength at Break, MD | 58.6 MPa | 8500 psi | ASTM D882 |
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |