Polymer Property : Film Tensile Strength at Break, MD = 8300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882, A
Total MDPE HL 323 Medium Density Polyethylene, Film Resin
Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
ExxonMobil EXACT™ 4053 Plastomer for Film Applications
Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
ExxonMobil HDPE HTA 001HP2 High Density Polyethylene (HMW) Resin
Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughn..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 ..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..
Film Tensile Strength at Break, MD 57.2 MPa
8300 psi
ASTM D882
Formosa Plastics Formolene® E927 Film HDPE
High Density Polyethylene High Molecular Weight Bi-Modal Resin For Thin Film Applications Formolene® E927 is a high molecular weight grade of HDPE designed for high drawdown to produce thin films w..