Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 56.5 MPa | 8190 psi | ASTM D882 |
ExxonMobil LL 1002.32 Cast Film Resin
(discontinued **) LL 1002.32 is a butene LLDPE resin designed for the cast film process. Films made from LL 1002.32 have very good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8190 psi | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8190 psi | |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8190 psi | |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |