Film Tensile Strength at Break, MD 30.0 - 45.0 MPa
4350 - 6530 psi
50% RH; DIN 53455
Stanelco Bioplast® GS 2189 Biodegradable Plastic
Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i..