Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882, A |
Total MDPE HL 323 Medium Density Polyethylene, Film Resin Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
ExxonMobil EXACT™ 4053 Plastomer for Film Applications Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
ExxonMobil HDPE HTA 001HP2 High Density Polyethylene (HMW) Resin Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughn.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | |
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 .. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Film Tensile Strength at Break, MD | 57.2 MPa | 8300 psi | ASTM D882 |
Formosa Plastics Formolene® E927 Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin For Thin Film Applications Formolene® E927 is a high molecular weight grade of HDPE designed for high drawdown to produce thin films w.. |