Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil LL 1002.32 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil LL 1002x74 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil LL 1002x79 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 730.09 is a 17.2% vinyl acetate copolymer film resin. LD 730.09 is designed to have superior strength and toughness combined with excellent optics and sealing ..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil LL 1002.09 Blown Film Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil LL 1002x75 Blown Film Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..