Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 51.4 MPa | 7450 psi | Calculated from mfr's report of 40.5 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® N196 Paper, 3 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Film Tensile Strength at Break, MD | 51.4 MPa | 7450 psi | |
Dow AFFINITY™ FM 1570 Polyolefin Plastomer AFFINITY® FM 1570 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide film products with excellent sealability and high hot tack strength, outstanding blown film optics, and .. |
|||
Film Tensile Strength at Break, MD | 51.4 MPa | 7450 psi | |
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of .. |
|||
Film Tensile Strength at Break, MD | 51.4 MPa | 7450 psi | |
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high .. |
|||
Film Tensile Strength at Break, MD | 51.4 MPa | 7450 psi | |
Dow Elite® 5110 Linear Low Density Polyethylene 5110 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers unique combination of high modulus and excellent impact strength, allowing for downgaugin.. |
|||
Film Tensile Strength at Break, MD | 51.4 MPa | 7450 psi | ASTM D882 |
LyondellBasell Alathon® L4434 High Density Polyethylene ApplicationsALATHON L 4434 is a medium molecular weight high density copolymer for use in blown film applications. Typical applications include blown film over pouches. Regulatory StatusL 4434 meet.. |