Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
ASTM D882
M. Holland Company MAGMA® LM115-B LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.
Film Tensile Strength at Break, MD 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D882
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Film Tensile Strength at Break, MD 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D882
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
ASTM D882
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin
Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation ..
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
510
ExxonMobil Hicor® 30 HT 103 OHD Film
One-side treated, non-sealable, oriented high density polyethylene film, which has outstanding stiffness, deadfold, and directional tear characteristics. This film has been designed to be used in va..
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
510
ExxonMobil Hicor® 30 HT 183 OHD Film
One-side metallized, non-sealable, oriented high density polyethylene film, which has outstanding deadfold and directional tear characteristics. This film has been designed to be used in various app..
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
ASTM D882
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin
LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
ASTM D882
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin
LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a..
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
ASTM D882
Dow INTEGRAL™ 936 High Heat Monolayer Adhesive Film
INTEGRAL 936 High Heat Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, cardboard, fi..
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
ASTM D882
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b..