Polymer Property : Film Tensile Strength at Break, MD = 4550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 31.4 MPa
4550 psi
500mm/min, Ultimate; ASTM D638
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical Properties Additives: Antiblocking agent, Slip AgentApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical
Film Tensile Strength at Break, MD 31.4 MPa
4550 psi
500mm/min, Ultimate; ASTM D638
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural Film, Shoe solesCSA No. 24937-78-8Information provided by LG Chemical
Film Tensile Strength at Break, MD 31.4 MPa
4550 psi
Ultimate; ASTM D882
LG Chemical SEETEC ST508 Linear Low Density Polyethylene, Cast Film Grade
Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica..