Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 234 - 303 MPa | 34000 - 44000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |
|||
Film Tensile Strength at Break, MD | 221 - 303 MPa | 32000 - 44000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film
(discontinued **) Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many .. |
|||
Film Tensile Strength at Break, MD | 234 - 303 MPa | 34000 - 44000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1200 Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1200 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Film Tensile Strength at Break, MD | 234 - 303 MPa | 34000 - 44000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1200M Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1200M is a 0.48 mil (12 micron) biaxially oriented nylon 6 film with a polymeric coating which provides enhanced adhesion to a variety of inks, coatings, and adh.. |
|||
Film Tensile Strength at Break, MD | 221 - 303 MPa | 32000 - 44000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Film Tensile Strength at Break, MD | 234 - 303 MPa | 34000 - 44000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd.. |
|||
Film Tensile Strength at Break, MD | 221 - 303 MPa | 32000 - 44000 psi | ASTM D882 |
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati.. |