Polymer Property : Film Tensile Strength at Break, MD = 440 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 440 MPa
63800 psi
ASTM D882
LG Chemical SEETEC R3420 Polypropylene, Random Copolymer
Features: Seetec R3420 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance..
Film Tensile Strength at Break, MD 440 MPa
63800 psi
ASTM D882
LG Chemical SEETEC R3450 Polypropylene Random Copolymer
Features: Seetec R3450 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance..