Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, MD = 4300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
M. Holland Company LL102 LLDPE  (discontinued **)
Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Medium SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c)..
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
Westlake Hifor Xtreme SC74840 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74840 linear low density polyethylene is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more c..
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
Westlake Mxsite LC78104 Polyethylene
Mxsite LC78104 polyethylene is recommended for the skin layers of cast stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling ..
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
Chevron Phillips MarFlex® 7109DL LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
ExxonMobil Escorene™ LD 708.62 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 708.62 is a 14.9% VA copolymer film resin. Film made from LD 708.62 exhibits good impact strength and superior heat sealabilty.Availability: Latin America, Nor..
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
M. Holland Company LL106 LLDPE  (discontinued **)
Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2..
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
Chevron Phillips MarFlex® 7109CL LLDPE Blown Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Copyright © lookpolymers.com All Rights Reserved