Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, MD = 39.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 39.3 MPa
5700 psi
ASTM D882
ExxonMobil Exceed™ 1518EC Tough Premium Film Resin  (discontinued **)
Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superi..
Film Tensile Strength at Break, MD 39.3 MPa
5700 psi
ASTM D882
Formosa Plastics Formolene® FORMAX® L91507A Film (Hexene Grade) LLDPE  (discontinued **)
Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. ..
Film Tensile Strength at Break, MD 39.3 MPa
5700 psi
ASTM D882
Formosa Plastics Formolene® FORMAX® L91507E2 Film (Hexene Grade) LLDPE  (discontinued **)
Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. ..
Film Tensile Strength at Break, MD 39.3 MPa
5700 psi
ASTM D882
Formosa Plastics Formolene® FORMAX® L91507H Film (Hexene Grade) LLDPE  (discontinued **)
Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. ..
Film Tensile Strength at Break, MD 39.3 MPa
5700 psi
ASTM D882
M. Holland Company MAGMA® LL1091-K LLDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Film Tensile Strength at Break, MD 39.3 - 53.1 MPa
5700 - 7700 psi
ASTM D882
Honeywell PMP Polymethylpentene Film  (discontinued **)
PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by..
Film Tensile Strength at Break, MD 39.3 MPa
5700 psi
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli..
Film Tensile Strength at Break, MD 39.3 MPa
5700 psi
ASTM D882
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b..
Copyright © lookpolymers.com All Rights Reserved