Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 25.7 MPa | 3730 psi | ASTM D882 |
ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
Film Tensile Strength at Break, MD | 25.7 MPa | 3730 psi | ASTM D882 |
ExxonMobil Pax-Plus™ 3208 Blown Film Resin Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform.. |
|||
Film Tensile Strength at Break, MD | 25.7 MPa | 3730 psi | |
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21.. |