Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 37.3 MPa | 5410 psi | |
Kuraray HYBRAR® CF3 Mono Layer Cast Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Film Tensile Strength at Break, MD | 37.3 MPa | 5410 psi | ASTM D882 |
Dow AFFINITY™ PF 1146G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for high speed packaging applications requiring low seal initiation temperature and good machina.. |
|||
Film Tensile Strength at Break, MD | 37.3 MPa | 5410 psi | |
Kuraray HYBRAR® BF1 Three Layer Blown Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber w.. |