Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 254.93 MPa | 36975 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 65 Gauge Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics.Teijin® Tetoron® G2 is available in the following variations:G2: Non-pretreatedG2N: Adhesion Pretreat.. |
|||
Film Tensile Strength at Break, MD | 254.93 MPa | 36975 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 80 Gauge Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics.Teijin® Tetoron® G2 is available in the following variations:G2: Non-pretreatedG2N: Adhesion Pretreat.. |
|||
Film Tensile Strength at Break, MD | 254.93 MPa | 36975 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 92 Gauge Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics.Teijin® Tetoron® G2 is available in the following variations:G2: Non-pretreatedG2N: Adhesion Pretreat.. |
|||
Film Tensile Strength at Break, MD | 254.93 MPa | 36975 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® O Polyester Film, 300 Gauge Teijin® Tetoron® O is the designation for a family of super clear polyester films. They have very smooth surface characteristics and are knurled. The combination of smoothness and knurling provide.. |
|||
Film Tensile Strength at Break, MD | 254.93 MPa | 36975 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® OX Polyester Film, 400 Gauge Teijin® Tetoron® O is the designation for a family of super clear polyester films. They have very smooth surface characteristics and are knurled. The combination of smoothness and knurling provide.. |
|||
Film Tensile Strength at Break, MD | 254.93 MPa | 36975 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 100 Gauge Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and.. |
|||
Film Tensile Strength at Break, MD | 254.93 MPa | 36975 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 150 Gauge Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and.. |
|||
Film Tensile Strength at Break, MD | 254.93 MPa | 36975 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 200 Gauge Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and.. |