Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
Westlake Mxsten CV77518 Polyethylene Plastomer Mxsten CV Plastomer CV77518 resin is a polyethylene plastomer designed for blown and cast film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a ve.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and streng.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
Formosa Plastics Formolene® L42009H Film (Butene Grade) LLDPE Butene Copolymer (Barefoot/with high AO)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administr.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
Formosa Plastics Formolene® L42009PE Film (Butene Grade) LLDPE Linear Low Density Polyethylene Butene Copolymer for Film Extrusion Formolene® L42009PE is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excell.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
Formosa Plastics Formolene® L42009A Film (Butene Grade) LLDPE Butene Copolymer (High Antiblock)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration a.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
Formosa Plastics Formolene® L42009B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
Formosa Plastics Formolene® L42009E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyo.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
Formosa Plastics Formolene® L42009M Film (Butene Grade) LLDPE Butene Copolymer (High slip and antiblock)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of poly.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil Escorene® LD 701.ID Blown Film Resin Escorene Ultra LD 701.ID is a fraction melt index, 10.5 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particularly.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5110 psi | |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Film Tensile Strength at Break, MD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil Escorene™ 768.MJ Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 768.MJ is a low gel 26.2% vinyl acetate copolymer designed for film and compounding applications. This resin provides very low modulus films with high tensile .. |