Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 32.8 MPa | 4750 psi | ASTM D882 |
Formosa Plastics Formolene® L62009A Film (Hexene Grade) LLDPE Hexene Copolymer (High Antiblock)Applications: Blown film applications that don’t require slip.Blown film applications that don’t require slip.Meets all requirements of the U.S. Food and Drug Admi.. |
|||
Film Tensile Strength at Break, MD | 32.8 MPa | 4750 psi | ASTM D882 |
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE Hexene Copolymer (High slip and antiblock)Applications: Blown film, general purpose filmBlown film, general purpose filmMeets all requirements of the U.S. Food and Drug Administration as specified i.. |
|||
Film Tensile Strength at Break, MD | 32.8 MPa | 4750 psi | ASTM D882 |
Formosa Plastics Formolene® L62009H Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Film Tensile Strength at Break, MD | 32.8 MPa | 4750 psi | ASTM D882 |
Formosa Plastics Formolene® L62009B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles.. |
|||
Film Tensile Strength at Break, MD | 32.8 MPa | 4750 psi | ASTM D882 |
Formosa Plastics Formolene® L62009X Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cross laminated filmCross laminated filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of.. |