Polymer Property : Film Tensile Strength at Break, MD = 3000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 20.7 - 42.7 MPa
3000 - 6190 psi
Average value: 30.6 MPa Grade Count:11
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
ExxonMobil ESCOR™ AT 320 Blown Film Resin  (discontinued **)
ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 20.7 - 31.7 MPa
3000 - 4600 psi
ASTM D882
Honeywell ACLAR® 33C (7.80 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
LyondellBasell Petrothene® NA942000 Low Density Polyethylene, Film Extrusion Grade
PETROTHENE NA942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone and agricultural and construction ma..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
LyondellBasell Petrothene® NA942094 Low Density Polyethylene
ApplicationsPETROTHENE NA 942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone, and agricultural and c..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade)
ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade)
ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
Westlake EF677 Low Density Polyethylene
Westlake EF677 is a high melt index LDPE resin suggested for garment films, or other applications requiring excellent drawdown. This material is also an excellent choice for PE foam applications.App..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin
Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
ExxonMobil LDPE LGA 105 Low Density Polyethylene Resin
Product Description: LGA 105 is a homopolymer, garment film resin with good toughness. It is capable of being draw-down to thin gauges.Availability: North America Additive: Antiblock: NoSlip: NoPro..
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Film Grade)
ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for..
Film Tensile Strength at Break, MD 20.7 - 55.5 MPa
3000 - 8050 psi
Average value: 41.4 MPa Grade Count:3
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..