Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Eastman 184MF Polyethylene Film
(discontinued **) Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Eastman 1840F Polyethylene
(discontinued **) Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Huntsman PE 1017 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Huntsman PE1020 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium impact strength and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 .. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Huntsman PE1023 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good draw down characteristics.Applications: Film extrusion: drum liners, hardware packaging, and refuse bags.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Huntsman PE1041 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good optical, medium impact strength, and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 2.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-C LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil.. |
|||
Film Tensile Strength at Break, MD | 20.0 - 310 MPa | 2900 - 45000 psi | Average value: 197 MPa Grade Count:3 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Film Tensile Strength at Break, MD | 20.0 - 35.0 MPa | 2900 - 5080 psi | 50% RH; DIN 53455 |
Stanelco Bioplast® GF 106 Biodegradable Plastic Bioplast 106 is a versatile soft product, suitable for blown film extrusion of completely biodegradable products. Many customers find it is a natural replacement for LDPE. Made from potato starch m.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1905F Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE, LLDPEContains 1500 ppm slip agent and 2600 ppm antiblocking agentRecommended Applications:General purpose bagVeg.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ISO 527-3 |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ISO 527-3 |
Borealis Himod™ FT7324 . LDPE for Film Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
ExxonMobil Optema® TC-110 Blown Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM-D882 |
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene TU3002 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties (dart drop and Elmendorf tear strength), and good processability. These qualities ensure the p.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM-D882 |
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad.. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Film Tensile Strength at Break, MD | 20.0 - 59.0 MPa | 2900 - 8560 psi | Average value: 30.1 MPa Grade Count:13 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Film Tensile Strength at Break, MD | 20.0 MPa | 2900 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Film Tensile Strength at Break, MD | 20.0 - 38.6 MPa | 2900 - 5600 psi | Average value: 27.6 MPa Grade Count:7 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |